Skip to main navigation Skip to search Skip to main content

Vibration reduction ability of polymers, particularly polymethylmethacrylate and polytetrafluoroethylene

  • SUNY Buffalo

Research output: Contribution to journalArticlepeer-review

37 Scopus citations

Abstract

The vibration reduction ability of thermoplastics (PMMA, PTFE, PA-66 and acetal) and of a thermoset (epoxy) was compared by dynamic flexural testing at ≤ 1.0 Hz. Among these polymers, PMMA exhibited the highest loss modulus, while PTFE exhibited the highest loss tangent. A synthetic rubber had an exceptionally low loss modulus, but an exceptionally high loss tangent. Epoxy and acetal exhibited the lowest loss tangent.

Original languageEnglish
Pages (from-to)423-426
Number of pages4
JournalPolymers and Polymer Composites
Volume9
Issue number6
DOIs
StatePublished - 2001