Solution-processed lanthanum zirconium oxide as a barrier layer for high Ic-coated conductors

  • Srivatsan Sathyamurthy
  • , Mariappan Paranthaman
  • , Lee Heatherly
  • , Patrick M. Martin
  • , E. D. Specht
  • , Amit Goyal
  • , Thomas Kodenkandath
  • , Xiaoping Li
  • , Martin W. Rupich
  • Oak Ridge National Laboratory
  • American Superconductor Corporation

Research output: Contribution to journalArticlepeer-review

25 Scopus citations

Abstract

High-quality lanthanum zirconium oxide (La2Zr2 O7 or LZO) films have been deposited and processed on Ni-W substrates using a sol-gel processing approach. It has been demonstrated that crack-free coatings with thicknesses up to 100 nm can be processed in a single step, while thicker coatings (200-225 nm) were processed using a multiple coating and annealing process. Using simulated metalorganic deposition (MOD)-YBa2Cu3 O7-δ (YBCO) processing conditions, the barrier properties of the sol-gel LZO coating with a thickness of 120 nm were found to be comparable to that of the standard 3-1ayer buffer stack deposited using physical vapor deposition. Secondary ion mass spectroscopy depth profile analysis of LZO films annealed in oxygen-18 shows that LZO effectively stops the diffusion of Ni within the first 80-100 nm. Using MOD processes, a CeO2 cap layer and superconducting YBCO layer were deposited on sol-gel LZO/Ni-W. For the first time, using such an all-solution conductor architecture, a critical current (Ic) of 140 A/cm with a corresponding critical current density (Jc) of 1.75 MA/cm2 has been demonstrated. Using a very thin Y2O3 seed layer (∼10 nm) deposited by electron beam evaporation; improved texture quality in the LZO layers has been demonstrated. The performance of the LZO deposited on these samples was evaluated using a sputtered CeO2 cap layer and MOD YBCO layer. Critical currents of up to 255 A/cm (3.2 MA/cm2) with 0.8-μm-thick YBCO films have been demonstrated, comparable to the performance of films grown using physical vapor deposited yttria stabilized zirconia as a barrier layer. Similar experiments using an MOD-CeO2 cap layer and MOD-YBCO layer yielded critical currents of 200 A/cm (2.5 MA/cm2) with 0.8-μm-thick YBCO films.

Original languageEnglish
Pages (from-to)910-914
Number of pages5
JournalJournal of Materials Research
Volume21
Issue number4
DOIs
StatePublished - Apr 2006

Fingerprint

Dive into the research topics of 'Solution-processed lanthanum zirconium oxide as a barrier layer for high Ic-coated conductors'. Together they form a unique fingerprint.

Cite this