Abstract
Nickel aluminide Ni3Al in the single phase form, with grain size ∼ 10 μm, porosity ∼ 5%, tensile strength 425 MPa, modulus 92 GPa and ductility 9.5% at room temperature, was fabricated by reactive infiltration at 800°C of liquid aluminium into a porous preform containing 78 vol % nickel and made by sintering 3-7 μm size nickel particles. Without sintering, the preform contained 58 vol % nickel and reactive infiltration resulted in an aluminium-matrix NiAl3 particle ( ∼ 50 μm size) composite and extensive growth of Ni-Al needles from the preform to the excess liquid aluminium around the preform.
| Original language | English |
|---|---|
| Pages (from-to) | 2117-2122 |
| Number of pages | 6 |
| Journal | Journal of Materials Science |
| Volume | 31 |
| Issue number | 8 |
| DOIs | |
| State | Published - 1996 |
Fingerprint
Dive into the research topics of 'Nickel aluminide (Ni3Al) fabricated by reactive infiltration'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver