Activated carbon filaments of diameter approximately 0.1 μm, main pore size (BJH) 55 angstroms, specific surface area 1310 m2/g and yield 36.2% were obtained by activating carbon filaments of diameter approximately 0.1 μm in CO2+N2 (1:1) at 970 °C for 80 min. Prior to this activation, the filaments were surface oxidized by exposure to ozone.