This study evaluated the fracture resistance of maxillary premolars with MOD cavity preparation and simulated periodontal ligament. The teeth were restored with silver amalgam (G1), Scotchbond Multi-Purpose Plus and silver amalgam (G2) and Panavia F and silver amalgam (G3). After restorations were made, the specimens were stored at 37°C for 24 hours at 100% humidity and submitted to the compression test in the Universal Testing Machine (Instron). The statistical analysis of the results (ANOVA and Tukey Test) revealed that the fracture resistance of group 2 (G2=105.720 kgF) was superior to those of groups 1 (G1=72.433 kgF) and 3 (G3=80.505 kgF) that did not differ between them.
| Original language | English |
|---|---|
| Pages (from-to) | 349-353 |
| Number of pages | 5 |
| Journal | Operative Dentistry |
| Volume | 27 |
| Issue number | 4 |
| State | Published - 2002 |
Fingerprint
Dive into the research topics of 'Fracture resistance of premolars with bonded class II amalgams'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver