An aqueous solution-based doping strategy for large-scale synthesis of Sb-doped ZnO nanowires

  • Fei Wang
  • , Jung Hun Seo
  • , Dylan Bayerl
  • , Jian Shi
  • , Hongyi Mi
  • , Zhenqiang Ma
  • , Deyin Zhao
  • , Yichen Shuai
  • , Weidong Zhou
  • , Xudong Wang
  • University of Wisconsin-Madison
  • University of Texas at Arlington

Research output: Contribution to journalArticlepeer-review

67 Scopus citations

Abstract

An aqueous solution-based doping strategy was developed for controlled doping impurity atoms into a ZnO nanowire (NW) lattice. Through this approach, antimony-doped ZnO NWs were successfully synthesized in an aqueous solution containing zinc nitrate and hexamethylenetetramine with antimony acetate as the dopant source. By introducing glycolate ions into the solution, a soluble antimony precursor (antimony glycolate) was formed and a good NW morphology with a controlled antimony doping concentration was successfully achieved. A doping concentration study suggested an antimony glycolate absorption doping mechanism. By fabricating and characterizing NW-based field effect transistors (FETs), stable p-type conductivity was observed. A field effect mobility of 1.2cm 2V- 1s- 1 and a carrier concentration of 6 × 1017cm- 3 were achieved. Electrostatic force microscopy (EFM) characterization on doped and undoped ZnO NWs further illustrated the shift of the metal-semiconductor barrier due to Sb doping. This work provided an effective large-scale synthesis strategy for doping ZnO NWs in aqueous solution.

Original languageEnglish
Article number225602
JournalNanotechnology
Volume22
Issue number22
DOIs
StatePublished - Jun 3 2011

Fingerprint

Dive into the research topics of 'An aqueous solution-based doping strategy for large-scale synthesis of Sb-doped ZnO nanowires'. Together they form a unique fingerprint.

Cite this